মেজারমেন্ট প্লাস / মাইনাস কি কি কারণে হয় এবং কি কি করলে মেজারমেন্ট প্লাস / মাইনাস হবে না.

 ★ Root Cause:

1) Fabric roll to roll shrinkage variation.

2) Lay time fabric tension tight or losseness in the table.

3) Fabric not proper relax.

4) Tension incorrect.

5) Handaling problem.

6) Excessive lay hight.

7) Lack of sincerity.

8) Poor fabric shrinkage.

9) Spreading machine speed not keep in right limitation.

10) After completing lay, air press not done  fulfill.

11) Fabric both side tight & middle losse / Fabric both side losse & middle tight.

12) Stripe / Yarn dyed Bowing Fabric cutting time, Stripe/ Yarn dyed counting both side ok but measurement discrivancy  found.

13) Same roll fabric but repeat measurement deviation.

★ Action Plan:

1) Shrinkage test must be of every batch within tolerance from every roll.

2) Tension tight or losseness fabric layed in the time table with soft handed.

3) Fabric must be proper way relax with required hours.

4) Fabric GSM wise spreading machine tension proper adjustment.

5) Motivation & Counselling to make sure proper handling.

6) Control lay height through proper SOP.

7) Enhance QC activities.

8) For poor fabric shrinkage pattern must be adjust, Shrinkage tolerance within buyer standard  required.

9) Spreading machine speed adjust by fabric type& gsm wise.

10) After the lay is complete, the air in the table should be left completely and then the lay should be pulled.

11) Tight or losseness fabric return to dyeing after re Prosess than cutting.

12) Bowing fabric cutting time needed extra care.

13) Same roll fabric but repeat wise cutting done. 



Comments